Visit http://www.esabna.com/ for more information about our products.

4 Steps To Proper Nozzle Selection

Print Print

 

  1. Choose One-Piece or Two-Piece Nozzle:
    Acetylene - one-piece nozzle always.
    Other Fuel Gases - two-piece nozzle provides most efficient operation for normal cutting. One-piece nozzle extends life where heating is very severe.
  2. Choose Series:
    OXWELD® 1500 Series Nozzles -
    CW-23, CW-400 and CW-500 Cutting Attachments
    C-32, C-66, C-77 and C-97 Hand Cutting Torches
    All Machine Cutting Torches
    PUROX® 4200 Series Nozzles -
    CW-200, CW-250, and CW-300 Cutting Attachments
    Type “E” and C-84 Hand Cutting Torches
  3. Choose Preheat Capacity: Choice of nozzle depends on preheat capacity. Steel coated with rust and scale, as well as bevel cutting, requires heavy preheat.
  4. Choose Size:
    Select size recommended for thickness of steel to be cut. Oversize nozzles waste gas. Use oxygen pressure recommended for nozzle.

Nozzle Selection

OXWELD® and PUROX® Cutting Nozzles

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages – permit re-dressing nozzle without affecting performance
  • One-piece nozzle is a single piece of solid copper – provides maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece nozzles – recommended for high efficiency with fuel gases other than acetylene – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost
  • Conical seats – instant aligning provides tight seal, prevents leaks around nozzle nut
Powered by CommonSpot