Product Name Output Current Cut Capacity Input Voltage Duty Cycle 1 or 3 Phase
ESAB Handy Plasma 125
HP 125
11A 1/8" 115 or 230 30% 1
ESAB Handy Plasma 380
HP 380
30A 3/8" 230 35% 1
ESAB Handy Plasma 550
HP 550
35A 1/2" 230 40% 1
ESAB PowerCut 650
PC 650
40A 5/8" 208, 230, 460 40% 1 & 3
ESAB PowerCut 875
PC 875
60A 7/8" 208, 230, 460, 575 60% 1 & 3
ESAB PowerCut 1250
PC 1250
70A 1 1/4" 208, 230, 460, 575 60-100% 1 & 3
ESAB PowerCut 1500
PC 1500
90A 1 1/2" 208, 230, 460, 575 40-60% 1 & 3