Visit http://www.esabna.com/ for more information about our products.

The Basics of Oxy-Fuel Cutting

Print Print

Q. What is Oxy-Fuel Cutting?
A. Oxy-fuel cutting is a chemical reaction between pure oxygen and steel to form iron oxide.
It can be described as rapid, controlled rusting.

Q. How does it work?
A. Preheat flames are used to raise the surface or edge of the steel to approximately 1800°F (bright red color). Pure oxygen is then directed toward the heated area in a fine, high pressure stream. As the steel is oxidized and blown away to form a cavity, the preheat and oxygen stream are moved at constant speed to form a continuous cut.

Q. Can I use oxy-fuel to cut any metal?
A. No. Only metals whose oxides have a lower melting point than the base metal itself can be cut with this process. Otherwise as soon as the metal oxidizes it terminates the oxidation by forming a protective crust. Only low carbon steel and some low alloys meet the above condition and can be cut effectively with the oxy-fuel process.

What Is Top Quality In Oxy-Fuel Cutting?
  1. Square top corner (with minimum radius)
  2. Cut face flat top to bottom (no undercut)
  3. Cut face square with respect to top surface
  4. Clean smooth surface with near vertical drag lines, and
  5. Little to no slag on bottom edge (easily removed by scraping)
Elements Of Oxy-Fuel Cutting

  • Preheat Flame
  • Oxygen Stream
  • Torch and Cutting Nozzle
  • Cutting Speed
  • Material Being Cut
Powered by CommonSpot