Alloy Surcharge Rates ($/Lb)
|
| Stainless Steel Alloy | Aug-03-09 | Sep-01-09 | Oct-06-09 | Nov-02-09 |
| 307 | $0.88 | $0.92 | $1.12 | $1.06 |
| 308, 308L, 308LSi, 308H | $1.04 | $1.08 | $1.30 | $1.20 |
| 309, 309L, 309LSi, 309LMo, 309Nb | $1.28 | $1.34 | $1.60 | $1.46 |
| 310, 310Mo, 310Cb | $1.54 | $1.64 | $2.00 | $1.80 |
| 312 | $0.96 | $1.02 | $1.30 | $1.22 |
| 316, 316L, 316LSi, 316H | $1.48 | $1.56 | $1.94 | $1.76 |
| 317, 317L | $1.58 | $1.68 | $2.08 | $1.90 |
| 320, 320LR | $2.40 | $2.58 | $3.00 | $2.70 |
| 347, 347H | $1.04 | $1.08 | $1.30 | $1.20 |
| 2209, 2509 | $1.46 | $1.50 | $1.94 | $1.84 |
| 410 | $0.28 | $0.26 | $0.30 | $0.30 |
| 410NiMo | $0.60 | $0.60 | $0.68 | $0.64 |
| 409Ti, 409Cb | $0.37 | $0.40 | $0.26 | $0.26 |
| 430LCb, 439Ti | $0.55 | $0.58 | $0.30 | $0.30 |
| 18CrCb | $0.56 | $0.58 | $0.48 | $0.48 |
| Nickel Alloy (covered electrode & cored wire) | ||||
| Nickel-Arc 55 & 550, Nicore 55, All-State 4-60, Super 4-60, 8-60, Corecast 8600 | $1.60 | $1.60 | $2.42 | $2.46 |
| Nickel-Arc 99, All-State 4IMP, #8 & Nickel NC | $2.62 | $2.62 | $4.06 | $3.80 |
| Arcaloy 112 & ENiCrMo-3 | $4.00 | $4.06 | $4.08 | $3.90 |
| ENiCrMo-6 | $4.25 | $5.50 | $5.38 | $5.02 |
| Arcaloy 8N12 | $2.20 | $2.22 | $3.30 | $3.20 |
| Arcaloy 9N10 | $2.38 | $2.40 | $3.34 | $3.26 |
| Arcaloy 276 | $5.24 | $5.26 | $5.24 | $4.16 |
| Nickel Alloy (solid bare wire) | ||||
| Nickel 55, All-State 4-60T | $2.00 | $2.02 | $3.10 | $2.98 |
| Nickel 99, All-State 4-T | $3.52 | $3.54 | $5.46 | $4.84 |
| Arcaloy ERNiCu-7 | $2.84 | $2.86 | $4.02 | $3.80 |
| Arcaloy 276 | $6.56 | $6.56 | $6.56 | $5.12 |
| Arcaloy 82 | $2.94 | $2.96 | $4.44 | $4.12 |
| Arcaloy 625 | $5.00 | $5.02 | $5.12 | $4.70 |