Unfortunately metal markets continue to force us to take the regrettable action of applying alloy surcharges. The surcharge will affect stainless and nickel steel filler metal products, namely covered electrodes, bare and cored wires. These rates will change monthly as market prices continue to vary. We understand the difficulty that raw material surcharges cause for our valued customers, however we feel this is the fairest way to deal with these extraordinary fluctuations in raw materials. Your continued cooperation and understanding is appreciated. Contact your local ESAB Territory Sales Manager for additional information.
Regards,
Marketing Department
Filler Metal Welding Consumables

  Stainless Steel Alloy   Aug-03-09   Sep-01-09   Oct-06-09   Nov-02-09
  307   $0.88   $0.92   $1.12   $1.06
  308, 308L, 308LSi, 308H   $1.04   $1.08   $1.30   $1.20
  309, 309L, 309LSi, 309LMo, 309Nb   $1.28   $1.34   $1.60   $1.46
  310, 310Mo, 310Cb   $1.54   $1.64   $2.00   $1.80
  312   $0.96   $1.02   $1.30   $1.22
  316, 316L, 316LSi, 316H   $1.48   $1.56   $1.94   $1.76
  317, 317L   $1.58   $1.68   $2.08   $1.90
  320, 320LR   $2.40   $2.58   $3.00   $2.70
  347, 347H   $1.04   $1.08   $1.30   $1.20
  2209, 2509   $1.46   $1.50   $1.94   $1.84
  410   $0.28   $0.26   $0.30   $0.30
  410NiMo   $0.60   $0.60   $0.68   $0.64
  409Ti, 409Cb   $0.37   $0.40   $0.26   $0.26
  430LCb, 439Ti   $0.55   $0.58   $0.30   $0.30
  18CrCb   $0.56   $0.58   $0.48   $0.48
  Nickel Alloy (covered electrode & cored wire)        
  Nickel-Arc 55 & 550, Nicore 55, All-State 4-60, Super 4-60, 8-60, Corecast 8600   $1.60   $1.60   $2.42   $2.46
  Nickel-Arc 99, All-State 4IMP, #8 & Nickel NC   $2.62   $2.62   $4.06   $3.80
  Arcaloy 112 & ENiCrMo-3   $4.00   $4.06   $4.08   $3.90
  ENiCrMo-6   $4.25   $5.50   $5.38   $5.02
  Arcaloy 8N12   $2.20   $2.22   $3.30   $3.20
  Arcaloy 9N10   $2.38   $2.40   $3.34   $3.26
  Arcaloy 276   $5.24   $5.26   $5.24   $4.16
  Nickel Alloy (solid bare wire)        
  Nickel 55, All-State 4-60T   $2.00   $2.02   $3.10   $2.98
  Nickel 99, All-State 4-T   $3.52   $3.54   $5.46   $4.84
  Arcaloy ERNiCu-7   $2.84   $2.86   $4.02   $3.80
  Arcaloy 276   $6.56   $6.56   $6.56   $5.12
  Arcaloy 82   $2.94   $2.96   $4.44   $4.12
  Arcaloy 625   $5.00   $5.02   $5.12   $4.70
         



Legal | Terms | SiteMap | ESAB Links | © 2005 ESAB Welding and Cutting Products. All rights reserved.


Mig Welders    |    TIG Welders    |    Arc Welders    |    Gas Welding & Cutting Equipment    |    Plasma Cutters
Welding Electrodes    |    Welding Wire

ESAB is the world's leading manufacturer of TIG welders, MIG or wire welders, stick welders, flux cored welders, multiprocess welders, plasma arc cutters, wire feeders, mutlioperator systems, automated welding systems, submerged arc welders, welding equipment, welding guns and accessories, oxyfuel torches, gas torches, gas regulators, gas welding tips and nozzles, stainless steel welding wire, flux cored welding wire, mig welding wire, welding consumables, and welder training materials for the Industrial, Maintenance & Repair, Farm and Ranch, Construction, Motorsports, Hobbyist and Fabrication markets.