| MIG(GMAW) | Current Range | Max Wire Feed Speed | AC Voltage | 1 or 3 Phase | ||||
|---|---|---|---|---|---|---|---|---|
| MigMaster 173 | 30-170 A | 670 ipm | 208(230) | 1 ph | ||||
| MigMaster 203 | 30-200 A | 670 ipm | 208(230) | 1 ph | ||||
| MigMaster 253 | 40-250 A | 748 ipm | 208(230) | 1 ph | ||||
| MigMaster 250 | 30-280 A | 650 ipm (16.5 m/m) | 208(575) | 1 ph | ||||
| MigMaster 275 | 30-280 A | 750 ipm (16.3 m/m) | 208(575) | 1 ph | ||||
| MultiMaster 160 | 5-160 A | 650 ipm (16.5 m/m) | 208(230) | 1 ph | ||||
| MultiMaster 260 | 35-300 A | 675 ipm (17.3 m/m) | 208(575) | 1 ph | ||||
| MultiMaster 300X | 35-300 A | 675 ipm (17.3 m/m) | 208(575) | 1 ph | ||||
| TIG(GTAW) | Current Range | Permitted Load | AC Voltage | 1 or 3 Phase | ||||
| CaddyTig 150 | 3-150 A | 35% @ 150A 60% @ 120A 100% @ 95A | 230 | 1 ph | ||||
| CaddyTig 200 | 3-200 A | 35% @ 180A 60% @ 140A 100% @ 110A | 230 | 1 ph | ||||
| Heliarc 161 AC/DC | 5-160 A | 40% @ 160A | 208(230) | 1 ph | ||||
| Heliarc 252 AC/DC | 5-320 A | 40% @ 280A | 208(575) | 1 ph | ||||
| Heliarc 352 AC/DC | 5-400 A | 40% @ 350A | 208(575) | 1 ph | ||||