AWS A5.20 E71T-1C/T-1M/T-9C/T-9M

Dual Shield 710X is an all-position flux cored wire for general purpose welding. It provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 710X can be used with either 100% CO2 or a 75/25 Argon CO2 gas mix, however pure CO2 is recommended in applications where weld joint restraint is high.

Applications include rail car, barges and general fabrication.