Welding
Non-Ferrous
Metals
Treating
Welding
Cast Iron
Welding
Ferrous
Metals
2
Continued
on next page...
Fig. 18-1.
Here is a large piston which
has been rough-turned in preparation
for bronze surfacing. Fig.
18-3. This 26-in. piston, with all grooves
filled and then overlaid, is ready
for machining. Fig.
18-2. As piston is rotated in a preheating
furnace, bronze is deposited
in the grooves. Fig.
18-4. This photograph shows a resurfaced
18-in. piston during the final