5 FILTER RECOMMENDATIONS (adapted from ANSI Safety Standard Z49.1) Application Mig (Gas Metal and Flux Cored Arc) Lens Shade No.* 60 to 160 amps 1 1 160 to 250 amps 1 2 250 to 500 amps 1 4 *As a rule of thumb, start with a shade that is too dark to see the arc zone. Then go to a lighter shade which gives sufficient view of the arc zone without exerting a strain on your eyes.