11 E71T-1M/T-9M (Dual Shield 7100 Ultra) ALL POSITION – This wire was formulated with a fast freezing slag that will support the molten weld puddle out of position. At low (140-200 amps) they exhibit good gap bridging characteristics necessary to weld poor fitup. At high amps (200-250 amps) they exhibit deep root penetration and can achieve higher out of position deposition rates than stick. This wire produces low fume generation. E81T1-Ni2 (Dual Shield 8000 Ni2) HIGH TOUGHNESS – ALL POSITION – These wires contain 2-3% nickel. They operate essentially the same as the E71T-1 all position wires they are derived from. The 2-3% nickel addition yields CVN toughness of 40-60 ft.-lbs. at 30-50 ft.-lbs. depending on shielding gas and cooling rates. Most of these wires will also maintain 70 ksi min. UTS after stress relief, making them useful in the vessel fabrication industry. This wire also meets AWS D.1.1 E8018-C1 chemical requirements for welding A242 and A588 weathering steels.