80 Typical
Undiluted Weld Metal Analysis (%) C
Mn
Si P
S
Al 0.22
0.34
0.28 0.012
0.007
1.3 Special
Precautions: Coreshield
40 contains fluoride compounds. The limit for fluorine may be reached before the
general fume limit
of 5 mg/m3 is reached. Consult MSDS for more
information. Standard
Diameters 1/16"
(1.6 mm), 5/64" (2.0 mm), 3/32" (2.4 mm), .120" (4.7 mm)
Recommended Welding Parameters page
95 Additional
Approvals page 117