45 CORE-BRIGHT®
Self Shielded Flux Cored Stainless
Steel Wires CORE-BRIGHT
is a flux cored self-shielding continuous wire designed to operate completely
open-arc. The careful
mixture of alloy and shielding agents in the core produces a weld deposit of excellent
appearance and radiographic quality.
The easily controlled arc and minimal spatter of this continuous feed
wire complement its characteristically
high deposition rate. The low weld penetration of CORE-BRIGHT
makes it a primary choice for overlay
or buildup applications. Penetration is sufficient also for joining like or
dissimilar metals. Rollover is minimized
by the viscous quality of the quick setting and easily removable
slag. Reduced cleaning time, high deposition,
and a self-shielding ability are all engineered into CORE-
BRIGHT to give maximum economy and
optimum efficiency in your welding operation. Operation
A constant voltage, direct current
generator or rectifier combined with gear type feed rolls produces best
results and is recommended.
Welding Current
DCEP (Electrode Positive)
Standard Diameters
0.045 (1.2mm), 1/16 (1.6mm),
5/64" (2.0mm), 3/32" (2.4mm)