44 Shield-Bright
X-tra Welding Parameters
and Deposition Data .045" (1.2 mm)
Amps 150
200 300
Volts 25
29 33
Wire Feed Speed in/min
259 410
860 (m/min)
(6.6) (10.4)
(21.9) Deposition
Rate lbs/hr 5.0
7.7 16.9
(kg/hr) (2.3)
(3.5) (7.7)
% Efficiency 83.9
84.2 87.0
1/16" (1.6 mm) Amps
200 240
400 Volts
25 28
33 Wire Feed Speed
in/min 172
225 495
(m/min) (4.4)
(5.7) (12.58)
Deposition Rate lbs/hr
6.7 8.1
18.9 (kg/hr)
(3.1) (3.7)
(8.6) % Efficiency
83.6 83.6
85.5 Electrical
Stick Out (ESO) is 1/2 - 1" (12.5 - 25 mm). DCEP
(Electrode Positive) is recommended. When using Ar/CO2
mixture, decrease voltage by as much as 2 volts.