28 Type
Specifications
Typical
Mechanical Properties Nickel-Arc
99 AWS A5.15
Tensile Strength, psi (MPa)
69,900 (482); Class
ENiCI-A Broke
in cast iron Hardness
in Weld 90-100
Rb AC/DCEP
Machinability
Excellent (Electrode
Positive) Color
Match Good
Nickel-Arc 99 is designed for welding
gray, malleable and nodular cast iron. The electrode utilizes a pure nickel core
wire. This is particularly
important when welding on overlay of cast iron where a high nickel deposit is
required. Machining is possible with this electrode.
Proper welding procedures should be followed. Nicore
55 Meets
Tensile Strength, psi (MPa)
73,300 (505) AWS
ENiFe-CI-A % Elongation
in 2" (51 mm) 12
Hardness (undiluted metal)
187 BHN DCEP
(Electrode Positive)
The Nicore 55 is a unique wire-within-a-wire
composite metal cored electrode developed to join or repair a variety of cast
irons. The deposit
consists of approximately 50.5% iron and 48% nickel, permitting expansion during
welding. Thermal stresses are minimized
due to the less frequent stops and starts previously associated with covered electrodes.
Operating on 98% argon/2% oxygen
shielding, this wire will produce a 97% deposition efficiency.
Recommended Welding Parameters page
29