15 Stub Loss Correction Table for Coated Electrodes 2" 3" 4" 5" Electrode         Deposition (50 m m ) (75 m m )        (100 m m )    (125 m m ) Length Efficiency STUB STUB STUB STUB 60.0% 50.0% 45.0% 40.0% 35.0% 12" 65.0% 54.2% 46.7% 43.3% 37.9% (300 mm) 70.0% 58.3% 52.5% 46.6% 40.8% Electrode 75.0% 62.5% 56.2% 50.0% 43.7% 80.0% 66.6% 60.0% 53.3% 46.6% 60.0% 51.4% 47.1% 42.9% 38.3% 14" 65.0% 55.7% 51.1% 46.4% 41.0% (350 mm) 70.0% 60.0% 55.0% 50.0% 45.0% Electrode 75.0% 64.3% 56.9% 53.6% 46.2% 80.0% 68.5% 62.8% 57.1% 51.4% 60.0% 53.3% 50.0% 46.6% 43.3% 18" 65.0% 57.7% 54.2% 50.5% 46.9% (450 mm) 70.0% 62.2% 56.3% 54.4% 50.5% Electrode 75.0% 66.6% 62.5% 56.3% 54.2% 80.0% 71.1% 66.6% 62.2% 57.7% Electrode Diameter Type Am ps 3/32 AC/DC 75 1.50 65% Lime 70 1.60 71% 1/8 AC/DC 100 2.07 65% Lime 100 2.42 71% 5/32 AC/DC 135 3.02 67% Lime 135 3.70 75% 3/16 AC/DC 160 3.88 75% Lime 160 4.35 78% 1/4 AC/DC 250 6.20 73% Lime 250 7.80 78% Deposition Rates and Efficiencies AC/DC and Lime Electrodes Deposition Rate - Efficiency
Electrodes
Covered
Stainless
Steel
Products
Solid Wire
& Rod
Products
ESAB
TIG & MIG
Wires
Cored
Wire
Products
Submerged
Arc
Products
Hard-
surfacing
Products
Calculations
Filler Metals
ASTM
Steels
Conversion
Tables
Arcaloy SS
Electrode Coat.
Arcaloy
Bare Wires
Arcaloy Metal
Core Wires
Nickel-Arc/
Nicore Cast Iron
Shield-Bright
Gas/Flux Cored
Core-Bright
Cored Wires