32 Electrode Storage Unopened containers can be stored safely for an indefinite length of time under normal dry storage conditions. They should be protected from humid air after the container is opened by being kept at 225°F to 300°F, (107°C to 149°C) or if the need arises, they can be reconditioned by baking for one hour at 700°F (371°C).