LESSON VII © COPYRIGHT 2000 THE ESAB GROUP, INC. DUAL SHIELD® LOW ALLOY FLUX CORED ELECTRODES SELECTOR GUIDE (Con't.) Dual Shield Typical Type AWS Class Category
As
Welded
Stress Relieved Weld Metal Analysis % Description-Applications Typical Properties Weld Metal Shielding Gas T-4130 CO2 C - 0.20 Mn - 1.10 AWS Si - 0.29 No Spec. Cr - 0.35 Ni - 1.25 Mo - 0.22 4130LN Argon- C - 0.22 25% CO2 Mn - 1.40 AWS Si - 0.52 No Spec. Cr - 0.56 Ni - 0.88 Mo - 0.18 88W CO2 Tensile Strength, psi 82,000 84,000 C - 0.05 Yield Strength, psi 68,000 70,000 Mn - 0.79 AWS Elongation %-2" 25 25 Si - 0.47 E80T1-W Reduction of Area % 65.7 56.5 Cr - 0.51 Charpy Impact 30  F 66 ft-lb 47 ft-lb Ni - 0.56                           0  F 42 ft-lb 35 ft-lb Cu - 0.55                        -20  F 32 ft-lb 23 ft-lb                        -44  F 20 ft-lb 20 ft-lb Coreweld W Argon- Tensile Strength, psi 92,500 C - 0.031 6% CO2 Yield Strength, psi 81,500 Mn - 1.33 AWS Elongation %-2" 26 Si - 0.43 E80C-G Charpy Impacts -20  F 38 Ni - 0.78                           -60  F 23.5 8100W CO2 Tensile Strength, psi 96,500 C - 0.05 Yield Strength, psi 89,500 Mn - 0.76 AWS Elongation %-2" 25 Si - 0.45 E80T1-W Reduction of Area % 61 Charpy Impacts 0  F 34                        -20  F 31 SEE CATALOG FOR COMPLETE PROPERTIES For flat and horizontal position welding of alloys such as A1S1 4130, 8630 and comparable types.  The heat treated properties will match those of the base metal. SEE CATALOG Metal cored electrode for weathering grade steels such as A588, A242, U.S.S. Cor- Tenfi , and Mayari Rfi . All-position flux cored electrode to provide color match for weathering grade steels. FOR COMPLETE PROPERTIES A basic slag electrode for flat and horizontal welding positions. Resists cracking and welds are of highest quality. For welding SAE 8630 and 4130 heat treatable steels. Low nickel content meets the standards of the National Association of Corrosion Engin For flat and horizontal position welding of the weathering grade steels such as Cor- Ten or Mayari R.













Lesson 1
The Basics of Arc Welding
Lesson 2
Common Electric
Arc Welding Processes
Lesson 3
Covered Electrodes for Welding
Mild Steels
Lesson 4
Covered Electrodes for Welding Low Alloy Steels
Lesson 5
Welding Filler Metals for Stainless Steels
Lesson 6
Carbon & Low Alloy
Steel Filler Metals -
GMAW,GTAW,SAW
Lesson 7
Flux Cored Arc Electrodes Carbon Low Alloy Steels
Lesson 8
Hardsurfacing Electrodes
Lesson 9
Estimating & Comparing Weld Metal Costs
Lesson 10
Reliability of Welding Filler Metals
Current
Chapter
Table of Contents
Go To Test
Print
Glossary
Search
Chapter
(Faster Download)
Turn Pages
Search
Document
(Slower Download)