© COPYRIGHT 2000 THE ESAB GROUP, INC. LESSON IV 4.6.10 Atom Arc 12018 (AWS E12018-M) - This electrode deposits high strength weld metal in both the as welded and stress-relieved conditions, which is required for welding many of the high strength quenched and tempered steels.  It is used to weld steels with 120,000 psi tensile  strength in applications, such as welding carbon and high strength alloy steel forgings for railroad equipment, high strength steel castings for structural work, and steel castings for highway bridges. Typical Mechanical Properties of Weld Metal Stress-Relieved As Welded 1 hr. @1025°F. Yield Point, psi 120,000 119,000 Tensile Strength, psi 132,000 129,000 % Elongation (2") 20 22 % Reduction of Area 56 60 Charpy V-Notch Impacts @72°F. 52 ft.-lbs. 54 ft.-lbs. @-60°F. 32 ft.-lbs. 31 ft.-lbs. Typical Chemical Composition of Weld Metal C Mn Si Cr Ni Mo 0.05% 1.90% 0.25% 0.85% 2.00% 0.50% 4.6.11 Atom Arc "T" (AWS E11018-M) - Atom Arc "T" electrodes were developed for welding U.S. Steels T-1 steel, which is quenched and tempered to high strength and ductility.  It has since been used to weld all of the quenched and tempered steels, including HY-80, the steel used for the pressure hulls of nuclear submarines. Typical Mechanical Properties of Weld Metal Stress-Relieved As Welded 1 hr. @1025°F. Yield Point, psi 103,000 102,000 Tensile Strength, psi 115,000 116,000 % Elongation (2") 22 24 % Reduction of Area 62 63 Charpy V-Notch Impacts @72°F. 80 ft.-lbs. 73 ft.-lbs. @0°F. 55 ft.-lbs. 50 ft.-lbs. @-40°F. 48 ft.-lbs. 42 ft.-lbs. @-60°F. 41 ft.-lbs. 26 ft.-lbs.





Lesson 1
The Basics of Arc Welding
Lesson 2
Common Electric
Arc Welding Processes
Lesson 3
Covered Electrodes for Welding
Mild Steels
Lesson 4
Covered Electrodes for Welding Low Alloy Steels
Lesson 5
Welding Filler Metals for Stainless Steels
Lesson 6
Carbon & Low Alloy
Steel Filler Metals -
GMAW,GTAW,SAW
Lesson 7
Flux Cored Arc Electrodes Carbon Low Alloy Steels
Lesson 8
Hardsurfacing Electrodes
Lesson 9
Estimating & Comparing Weld Metal Costs
Lesson 10
Reliability of Welding Filler Metals
Current
Chapter
Table of Contents
Go To Test
Print
Glossary
Search
Chapter
(Faster Download)
Turn Pages
Search Document
(Slower Download)