© COPYRIGHT 2000 THE ESAB GROUP, INC. LESSON IV 4.6.4 Atom Arc 8018CM (AWS E8018-B2) - This 1-1/4% chrome, 1/2% moly electrode deposits weld metal that retains high strength at temperatures up to 600°F.  The 8018CM electrodes are used to weld the 1/2% chrome-1/2% moly, 1% chrome-1/2% moly steels, as well as the 1-1/4% chrome-1/2% moly power piping, boiler tubing, plates and castings.  Many of the fossil fired steam boilers in electric generating plants in the United States have been welded with this electrode and its relative 9018CM. Typical Mechanical Properties of Weld Metal Stress-Relieved Stress-Relieved 8 hrs. @1150°F. 8 hrs. @1350°F. Yield Point, psi 82,400 63,800 Tensile Strength, psi 100,000 78,300 % Elongation (2") 23 32 % Reduction of Area 60.7 79.1 Charpy V-Notch Impacts @30°F. 64 ft.-lbs. 127 ft-lbs. Typical Chemical Composition of Weld Metal C Mn Si Ni Mo 0.06% 1.10% 0.40% 1.00% 0.50% 4.6.5 Atom Arc 8018W (AWS E8018-G) - The balanced alloy combination of chromium, nickel and copper of this electrode causes the weld metal to "weather" similarly to the weathering grade steels when exposed to the atmosphere.  The inform color blend of this weld metal with the weathered steel makes these electrodes the ideal choice when architectural appearance and weld integrity is important. Typical Mechanical Properties of Weld Metal Stress-Relieved As Welded 1 hr. @1025°F. Yield Point, psi 84,600 79,100 Tensile Strength, psi 94,400 90,100 % Elongation (2") 27 28 % Reduction of Area 68.8 72.3 Charpy V-Notch Impacts @-60°F. 63 ft-lbs. 44 ft.-lbs. Typical Chemical Composition of Weld Metal C Mn Si Ni Mo 0.05% 1.11% 0.32% 1.70% 0.28%





Lesson 1
The Basics of Arc Welding
Lesson 2
Common Electric
Arc Welding Processes
Lesson 3
Covered Electrodes for Welding
Mild Steels
Lesson 4
Covered Electrodes for Welding Low Alloy Steels
Lesson 5
Welding Filler Metals for Stainless Steels
Lesson 6
Carbon & Low Alloy
Steel Filler Metals -
GMAW,GTAW,SAW
Lesson 7
Flux Cored Arc Electrodes Carbon Low Alloy Steels
Lesson 8
Hardsurfacing Electrodes
Lesson 9
Estimating & Comparing Weld Metal Costs
Lesson 10
Reliability of Welding Filler Metals
Current
Chapter
Table of Contents
Go To Test
Print
Glossary
Search
Chapter
(Faster Download)
Turn Pages
Search Document
(Slower Download)