17
Diameters and Recommended Amperages
3/32" (2.4 mm)35-80
1/8" (3.2 mm)60-125
5/32" (4.0 mm)90-160
Identification
All-State Steelarc®
80LV printed on the electrode coating and package. Packaging
All sizes in 5-lb. (2.27 kg) and 10-lb.(4.54
kg) containers. ALL-STATE
Steelarc® 80 LV Red
Typical Application: Steel piping and
out of position welding.