8
Sizes 1/16"
(1.6mm) in coils. 1/16" (1.6mm) x 18" (450mm) bare only.
Identification
All-State®
111 printed on package. Packaging
1/16" (1.6mm) in 1-lb. (.45 kg), 4-oz.
(.11 kg) and 2-oz. (.06 kg) coils, and 2-oz. (.06 kg) Silver Kits with flux jars.
1/16" (1.6mm)
x 18" (450mm) rods in 1-lb. (.45 kg) packages and 4-oz. (.11 kg) tubes.
ALL-STATE®
111 Typical Application:
Repair of electrical controls, switches. *NOTE:
Do not use on food processing and handling equipment.