6 Size: 1/16" (1.6mm) in coils. Identification All-State® 107 printed on package. Packaging 1/16" (1.6mm) on 1-lb. (.45 kg) spools and in 2-oz. (.06 kg) Silver Kits with flux jars. ALL-STATE® 107 Typical Application: Joining aluminum cable to copper lugs.