4 Sizes
1/16" (1.6mm) in coils. 1/16" (1.6mm)
and 3/32" (2.4mm) x 18" (450mm)bare or flux coated (TRUCOTE®).
Identification
All-State®
101 or 101FC printed on package. Flux coated rods have blue colored coating.
Packaging 1/16"
(1.6mm) in 1-lb. (.45 kg) coils. 1/16" (1.6mm) in 4-oz. (.11 kg) and 2-oz. (.06
kg) coils, and 4-oz. (.11 kg) and 2-oz.
(.06 kg) Silver Kits with flux jars. 1/16" (1.6mm) and 3/32" (2.4mm) x 18" (450mm)
bare or flux coated rods in 1-lb.
(.45 kg) packages and 4-oz. (.11 kg) tubes. *NOTE:
Contains cadmium. Do not use on food processing and handling
equipment. Cadmium free available upon request. ALL-STATE®
101 Typical Application:
T joints.