13 Sizes 1/32" (.8mm), 3/64" (1.2mm), 1/16" (1.6mm), 3/32" (2.4mm) and 1/8" (3.2mm) solid wire. Acid and Rosin flux cored wire is available, contact customer service for price and delivery. Identification All-State® 430 printed on spools and packages. Packaging All wire sizes on 1-lb. (.45 kg) spools. 1/16" (1.6mm) size in Dynagrip® Solder Kit (solder and flux). *Also available in cadmium free paste form. ALL-STATE® 430 Typical Application: Stainless steel equipment repair.