2 ALL-STATE® 31 Typical Application: Aluminum tubing. Sizes 1/16" (1.6mm), 3/32" (2.4mm) and 1/8" (3.2mm) x 18" (450mm) Identification All-State® 31 or 31FC printed on package. Cream color on tip of 31 bare rod. Packaging 1/16" (1.6mm) in 1-lb. (.45 kg) and 5-lb. (2.27 kg) containers. All other sizes in 5-lb. (2.27 kg) containers