11 Sizes 1/16" (1.6mm) and 1/8" (3.2mm) solid wire. Identification All-State® 509 printed on spools and packages. Packaging All sizes on 1-lb. (.45 kg) and 5-lb. (2.27 kg) spools. 1/16" (1.6mm) size in Strongset® No. 509 Solder Kit (solder and flux). ALL-STATE Strongset® 509 Solder (Not for food handling equipment). Typical Application: General purpose, high strength aluminum soldering. Refrigeration Repairs Aluminum Coil Repair