2 ALL-STATE®
20 Typical Application:
Propellers, copper base metals, and many ferrous metals.
Diameter and Recommended Amperages
1/8" (3.2mm)90-125
5/32" (4.0mm)120-150
Identification
All-State®
20 printed on package. Packaging
All sizes in 10-lb. (4.54 kg) containers.
*Also available in MIG in .045" (1.1mm)
and 1/16" (1.6mm) x 25 lb. (11.34 kg) spools and TlG in 1/16" (1.6mm) and 3/32"
(2.4mm) x 36"
(900mm).