5
Identification
All-State®
Air Hardening printed on electrode coating and package. Packaging
3/32" (2.4mm) x 14" (350mm) in 5-lb.
(2.27 kg) containers. Other sizes in 10-lb. (4.54 kg) containers.
TERMPERING TEMPERATURES
0F.
CURVE IS WELD DEPOSIT TEMPERED
FROM "AS WELDED"
The tempering curves of the air hardening
die steels and the high carbon/high chrome
die steels all lie within the black shaded area.