ALL-STATE® Water Hardening Typical Application: Facing of Gear Teeth. Identification All-State® Water Hardening printed on electrode coating and package. Packaging 3/32" (2.4mm) x 9" (225mm) in 5-lb. (2.27 kg) containers. Other sizes in 10-lb. (4.54 kg) containers. *Also available in MIG and TIG TERMPERING TEMPERATURES 0F. CURVE IS WELD DEPOSIT TEMPERED FROM "AS WELDED" The tempering curves of all water hardening tool steels, including finishing steels, tool alloys, and chisel steels, lie within the black shaded area.