8 Diameters
and Recommended Amperages 3/32"
(2.4mm)50-90 1/8"
(3.2mm)80-120 5/32"
(4.0mm)110-150 3/16"
(4.8mm)130-170 Identification
All-State®
4-60 printed on electrode coating and package. Packaging
3/32" (2.4mm) x 9" (225mm) in 5-lb.
(2.27 kg) containers. 1/8" (3.2mm) and 5/32 (4.0mm) in 5-lb. (2.27 kg) and
10-lb. (4.54 kg) containers. 3/16"
(4.8mm) in 5-lb. (2.27 kg) container. ALL-STATE®
4-60 A premium
ferro-nickel all position electrode. Typical Application: Oil pans and cylinder
heads. *Also
available in TIG (4-60T)