4 Diameters
and Recommended Amperages 3/32"
(2.4mm)40-80 1/8"
(3.2mm)70-110 5/32"
(4.0mm)100-140 Identification
All-State®
4 IMP printed on electrode coating and package. Packaging
3/32" (2.4mm) x 9" (225mm) in 5-lb.
(2.27 kg) containers. Other sizes in 5-lb. (2.27 kg) and 10-lb. (4.54 kg) containers.
*Also available in TIG (4-T)
ALL-STATE®
NO. 4 IMP Typical
Application: Engine blocks and cylinder heads. Also ideally suited
for machine parts and pump housings.