4 All-State® No. 31FC and 31 Paste Syringe Non-corrosive, non-hygroscopic flux inside a tubular rod; no separate flux required. For joining light gauge aluminum as used in furniture, truck and trailer bodies, window frames, aircraft instruments. Excellent color match but will darken if anodized. Very fluid, capillary action similar to silver brazing alloys. 1/16" and 3/32" diameter x 18" length in 1lb., 4 oz. and 2 oz. tubes, 1/16" also in 4-ft. coil in a plastic vial. Also available in paste form in 2 oz. syringes - 10 syringes per Display Case.