9
All-State®
Chemical Aids All-State
Galvover® Spray
A zinc rich protective spray for metal
surfaces subject to rust. Provides great protection against salt corrosion.
Packaged in 16 oz. cans, 12 to a case.
All-State®
Anti-Spatter Spray A
quickly applied weld spatter preventive spray. Spatter around weld beads, jigs,
and fixtures is virtually eliminated.
Packaged in 16 oz. cans, 12 to a case.
All-State®
Nozzle-Gel Ice-blue
colored gel helps eliminate weld spatter buildup up on gas nozzles and contact
tubes. Provides better control
of gas shielding. Packaged
in 16 oz. jars, 12 to a case.